About this video
Stronger prints with the same filament
Most people make a part stronger by raising the infill percentage, which costs filament and print time. Fill multiline takes a different route. It prints every infill line as two, three or more lines side by side and spreads the pattern out to match, so the infill density and the filament used stay the same. You get fewer infill walls, but each one is much thicker.
In the video, two 15% Grid test squares come off the same printer. The one on the default setting is a fine mesh of single lines. The one with Fill multiline turned up is a coarse grid of thick walls, printed with the same amount of filament.
Where to find Fill multiline
The setting sits in the same place in Bambu Studio and OrcaSlicer.
| Step | Where to click |
|---|---|
| 1 | Open the Strength tab in the process settings |
| 2 | Find the Sparse infill section |
| 3 | Look for Fill multiline, right below Sparse infill density |
| 4 | Raise it from 1 to 2 or 3, then slice and print |
If you can't see it, check your infill pattern and density. Bambu Studio only shows Fill multiline when the sparse infill density is above 0% and the pattern supports it. Updating to a recent slicer version also helps, since it is a newer setting.
What the number does
| Fill multiline | What prints | When to use it |
|---|---|---|
| 1 (default) | One line per infill path | Everyday parts |
| 2 | Two lines side by side, pattern spaced twice as wide | Parts that feel soft at low infill |
| 3 | Three lines side by side, pattern spaced three times as wide | Brackets, mounts and parts that carry load |
| 4 and up | Very thick, widely spaced infill walls | Special cases only, see the warnings below |
OrcaSlicer's documentation says it keeps the cross-section of the infill constant for the density you set, so 15% with 3 lines is still 15%. It also notes that some other slicers simply multiply the lines, which would turn 15% into 45%. Compare the filament estimate in the slice preview before and after you change the setting to see what your slicer does.
Why thicker infill walls make a stronger part
A wall three lines thick is far stiffer than a single line, so the same plastic resists bending and crushing better. OrcaSlicer lists these uses for multiline infill:
- Making parts stronger without adding material, usually with 2 or 3 lines.
- Stiffening weak, fast patterns like Lightning.
- Gears and other mechanisms, since thicker infill transfers torque better.
- Materials that need a minimum wall or infill thickness, like some flame-retardant PC, without going to 100% infill or a bigger nozzle.
Which infill patterns support it
In Bambu Studio the option appears for Grid, Cubic, Rectilinear, Aligned Rectilinear, Gyroid, Honeycomb, 3D Honeycomb, Adaptive Cubic, Support Cubic and Lightning. OrcaSlicer supports multiline on most of its patterns and lists them in its infill pattern reference. If you are not sure which pattern to pick in the first place, start with our infill pattern guide or the infill cheat sheet.
Print time depends on the pattern
Fill multiline doesn't add filament, but it can change print time. OrcaSlicer ran an infill analysis across its patterns:
| Pattern type | Effect of multiline on infill print time |
|---|---|
| Curved patterns (Gyroid, Honeycomb, 3D Honeycomb) | 15–21% faster with 2 lines, 23–32% faster with 3 |
| Crossing patterns (Grid, Cubic, Triangles) on the default strategy | 21–87% slower, because the paths turn back at every crossing |
| Crossing patterns on the Crossing strategy (newer OrcaSlicer builds) | Within about 2% of a single line |
The longer, gentler paths of Gyroid and Honeycomb mean fewer slowdowns, which is why they get faster. If you want strength and speed together, pair Fill multiline with Gyroid.
Things to watch out for
- Top surfaces. Thicker, more widely spaced infill leaves bigger gaps for the top layers to bridge. If you see pillowing or holes on the top, add one more top shell layer. Our guides on fixing bad top layers and the one simple top layer test cover the rest.
- More than 3 lines on crossing patterns. With the Crossing strategy in OrcaSlicer, walls of more than 3 lines overlap over a large area at every crossing. That can over-extrude and make the nozzle scrape the infill, and OrcaSlicer warns about it when it slices. Stay at 2 or 3, or use a pattern whose lines don't cross. The video uses 4 on Grid to make the difference easy to see.
- Walls still matter most. Infill helps, but wall count does more for strength than anything else. See the one setting for 3D printing strength.
Quick settings recap
| Setting | Value |
|---|---|
| Location | Strength > Sparse infill > Fill multiline |
| Starting value | 2 or 3 |
| Best paired pattern | Gyroid or Honeycomb |
| Infill density | Keep what you normally use, for example 15% |
| If the top surface looks rough | Add one top shell layer |
More ways to make prints stronger
- How to make 3D prints stronger in the slicer with Gyroid, extra walls and a hotter nozzle.
- Day 3 of Learn 3D printing in 7 days walks through walls, shells and infill.
- Make prints stronger in specific spots with a modifier.
- What different infill percentages look like inside a print.
FAQ
Does Fill multiline use more filament?
In Bambu Studio and OrcaSlicer, no. They spread the pattern out so the density and the filament stay the same. Compare the filament estimate in the slice preview to confirm it for your version.
What number should I set Fill multiline to?
Start with 2 or 3. That gives a noticeably stiffer part without the over-extrusion risk of more lines at the crossings of patterns like Grid.
Is Fill multiline better than raising the infill percentage?
It makes the part stiffer without using more filament, while raising the percentage adds filament and time. For the most strength, add walls first, then use Fill multiline.
Why can't I see Fill multiline in my slicer?
Your infill pattern may not support it, or the infill density is 0%. Switch to a pattern like Gyroid or Grid and update to a recent version of Bambu Studio or OrcaSlicer.
Does Fill multiline make prints slower?
It depends on the pattern. In OrcaSlicer's tests Gyroid and Honeycomb printed faster with 2 or 3 lines, while Grid and Cubic on the default strategy printed slower.
3 best slicer hacks you should know: OrcaSlicer plugins
Autoplay paused while you read — scroll back up to continue
Stronger 3D prints with one slicer setting: Fill multiline
Fill multiline prints every infill line as 2 or 3 lines side by side at the same density, so parts get stiffer without extra filament. Where to find it in Bambu Studio and OrcaSlicer, and when to use it.